MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M RPF-C (0.32 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: 3M™ RPF-C (Reinforced Polyurethane Foam) is a polyurethane foam with layers of continuous strand fiberglass throughout the polyurethane matrix. The composites are 37% to 60% lighter than plywood, dimensionally stable, very low water absorption (0.75% or less) and will not have any water rot or insect infestation.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.75 %0.75 %ASTM C272
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 13.09 MPa1898 psiASTM D790
Flexural Modulus 0.525 GPa76.1 ksiASTM D790
Compressive Strength 2.96 MPa429 psiCore; ASTM C365
Compressive Modulus 0.05187 GPa7.523 ksiCore; ASTM C365
Shear Modulus 0.03527 GPa5.115 ksiCore; ASTM C273
Shear Strength 2.36 MPa342 psiCore; ASTM C273

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M RPF-C (0.24 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks
General Plastics LAST-A-FOAM® TR-20 Polyurethane Foam
ITW Insulation TRYMER® 200L Polyisocyanurate Foam
J6 Polymers JFOAM™ BX-190 Engineered Specialty Foam

PMM34781 / 169528

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.