MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay BR® 623P4 Potting Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: BR® 623P4 is a one-part epoxy material designed for use in insert or edge filling of honeycomb structures. It has been formulated to offer the benefit of low viscosity, making it especially suitable for hand filling of small cell size [1/8 inch (3.175 mm)] and deep section [> 1 inch (> 25.4 mm)] honeycomb core and for applications with automated pumping or dispensing equipment. The long working out-life of BR 623P4 at room temperature eliminates the need for cleaning out pumping equipment pipe work with solvent materials. The low cured density (0.70 g/cm2) and high mechanical performance of BR 623P4 allows for excellent specific properties in honeycomb structures. The thixotropic nature of BR 623P4 ensures that there is no slump of the potting compound when used for edge filling of honey comb panels.

Features & Benefits:

  • Low odor
  • No slump during cure
  • -67°F to 230°F (-55°C to 110°C) service temperature
  • Specific gravity of 0.70 ± 0.05
  • Co-curable with most 250°F to 350°F (121°C to 177°C) advanced composite materials
  • Flammability: Self-extinguishing
  • Smoke density: passes JAR/FAR 25.853 part V
  • Resistant to aerospace fluids and solvents
Suggested Applications:
  • Insert or edge filling of honeycomb structures

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %
Storage Temperature <= -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 49.0 MPaBlock, 70°C/70% RH
 52.0 MPaBlock, Distilled water at 23°C
 52.0 MPaBlock, Jet fuel3 at 23°C
 54.0 MPaBlock, Hydraulic fluid2 at 23°C
 57.0 MPaBlock, Dry heat at 80°C
 42.0 MPa
@Temperature 80.0 °C
Block
 53.0 MPa
@Temperature 23.0 °C
Block
 66.0 MPa
@Temperature -55.0 °C
Block
Compressive Modulus 2600 MPa
@Temperature 80.0 °C
Block
 3200 MPa
@Temperature 23.0 °C
Block
 3300 MPa
@Temperature -55.0 °C
Block
Shear Strength 2700 psi
@Temperature 80.0 °C
Block
 3300 psi
@Temperature -55.0 °C
Block
 3800 psi
@Temperature 23.0 °C
Block
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 110 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
ColorPale Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dymax 3069P Fast Shallow Potting Compound and Sealant
CHT Group QSil 7720 Addition Cure Potting Material
CHT Group QSil 562 Addition Cure Potting Material
CHT Group QSil 550R QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 430 QSI Quantum Silicones Silicone Potting Material

PCYTED005 / 180307

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.