MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

CHT Group QSil 562 Addition Cure Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 562 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readily repairable and has a 150°C RTI rating.

Key Features:

  • 100% solids - no solvents
  • Fast curing
  • Low modulus
  • Good elongation
  • 150°C RTI rating
  • UL-94 V-0

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccUncatalyzed, QSil 562A
 1.60 g/cc1.60 g/ccUncatalyzed, QSil 562B
Viscosity 4500 cP4500 cPUncatalyzed, QSil 562B
 6000 cP6000 cPUncatalyzed, QSil 562A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060Cure 15 minutes at 150°C
Tensile Strength 1.72 MPa250 psiCure 15 minutes at 150°C
Elongation at Break 100 %100 %Cure 15 minutes at 150°C
Tear Strength 3.51 kN/m20.0 pliCure 15 minutes at 150°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Dielectric Constant 3.5
@Frequency 1000 Hz
3.5
@Frequency 1000 Hz
Dissipation Factor 0.00200.0020
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.620 W/m-K4.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 240 °C464 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 150 °C
0.250 hour
@Temperature 302 °F
As Tested
Pot Life 90.0 min90.0 min
Gel Time 240 min240 minCatalyzed
 
Descriptive Properties
ColorBeigeUncatalyzed, QSil 562B
 Dark GrayUncatalyzed, QSil 562A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QSil 550R QSI Quantum Silicones Silicone Potting Material
Henkel Loctite® 3180 Deep Potting Polyurethane
CHT Group QSil 13 Clear, Low Viscosity, Condensation Cure, Liquid Silicone Material for Coating and Potting Applications
Dymax 3069P Fast Shallow Potting Compound and Sealant
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material

PACC2100 / 199488

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.