MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Characteristics: superior wear resistance, hardenable, excellent corrosion resistance.

Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for oil well pumps, separating screens and strainers, springs, shears, and wear surfaces.

Information provided by Allegheny Ludlum

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.72 g/cc
Density 7.68 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 93
Hardness, Rockwell C 29Hardened+Tempered 1200°F
 43Hardened+Tempered 1000°F
 50Hardened+Tempered 550°F
 52Hardened+Tempered 900°F
 53Hardened+Tempered 600°F
 53Hardened+Tempered 800°F
 53Hardened+Tempered 400°F
Tensile Strength, Ultimate 593 MPaAnnealed, Fine blanking quality
 648 MPaAnnealed
 936 MPaHardened 1900°F, Tempered 1200°F
 1434 MPaHardened 1900°F, Tempered 1000°F
 1619 MPaHardened 1900°F, Tempered 900°F
 1690 MPaHardened 1900°F, Tempered 600°F
 1729 MPaHardened 1900°F, Tempered 550°F
 1759 MPaHardened 1900°F, Tempered 800°F
 1868 MPaHardened 1900°F, Tempered 400°F
Tensile Strength, Yield 743 MPaHardened 1900°F, Tempered 1200°F
 1218 MPaHardened 1900°F, Tempered 1000°F
 1351 MPaHardened 1900°F, Tempered 600°F
 1360 MPaHardened 1900°F, Tempered 550°F
 1368 MPaHardened 1900°F, Tempered 900°F
 1385 MPaHardened 1900°F, Tempered 400°F
 1452 MPaHardened 1900°F, Tempered 800°F
 310 MPa
@Strain 0.2 %
Annealed, fine blanking quality
 379 MPa
@Strain 0.2 %
Annealed
Elongation at Break 24 %Annealed
 25 %Annealed, Fine blanking quality
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000610 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.6 µm/m-°C
@Temperature 20.0 - 200 °C
 12.8 µm/m-°C
@Temperature 20.0 - 600 °C
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 24.2 W/m-K
@Temperature 100 °C
Melting Point 1427 - 1510 °C
Solidus 1427 °C
Liquidus 1510 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.50 - 0.55 %
Chromium, Cr 13 - 14 %
Iron, Fe 81.7 - 85.7 %as balance
Manganese, Mn <= 1.0 %
Molybdenum, Mo 0.80 - 1.2 %
Nickel, Ni <= 0.50 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %
 
Descriptive Properties
Corrosion Rate mils per year0.593 (5% Phosphoric Acid at 49°C)Hardened martensitic grades were tested after tempering at 204°C
 4.79 (5% Acetic Acid at 49°C)Hardened martensitic grades were tested after tempering at 204°C
Pitting Potential, Volts vs. Sat. Calomel Electrode0.619100 ppm Chloride solution at 24°C, pH5, ground surface. Hardened martensitic grades were tested after tempering at 204°C.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
444 Ferritic Stainless Steel, 18Cr-2Mo (UNS S44400)
AK Steel 444 Ferritic Stainless steel
ATI Allegheny Ludlum 430 Ferritic Stainless Steel
Kinetics MIM 440C Stainless Steel
Eagle Brass 430 Ferritic Stainless Steel, Annealed

NL1036 / 17804

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.