MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eagle Brass 430 Ferritic Stainless Steel, Annealed
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical product applications include automotive trim and molding, dishwashers, range hoods, steam iron bases, and flatware and restaurant equipments.

Information provided by Eagle Brass Company

Key Words: UNS S43000; ASTM A240
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.70 g/cc0.278 lb/in³As Annealed
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 448 MPa>= 65000 psi
Tensile Strength, Yield >= 207 MPa>= 30000 psi0.2% Offset
Elongation at Break >= 20 %>= 20 %in 2 inches
Tensile Modulus 200 GPa29000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.9 µm/m-°C
@Temperature 20.0 - 649 °C
6.60 µin/in-°F
@Temperature 68.0 - 1200 °F
Thermal Conductivity 26.1 W/m-K181 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.12 %<= 0.12 %
Chromium, Cr 16 - 18 %16 - 18 %
Iron, Fe 79.81 - 84 %79.81 - 84 %Calculated as Balance
Manganese, Mn <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel 430 Ferritic Stainless steel
430 Stainless Steel annealed sheet
ATI Allegheny Ludlum 430 Ferritic Stainless Steel
430 Stainless Steel annealed at 815°C
AISI Type 430F Stainless Steel

NEAGLE549 / 147526

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.