MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 4200 Marine Adhesive/Sealant Fast Cure
Categories: Polymer; Adhesive

Material Notes: A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds to wood, gelcoat and fiberglass. It forms watertight, weather-resistant seals on joints and boat hardware above and below the waterline. In addition, its flexibility allows for dissipation of stress caused by shock, vibration, swelling or shrinking.

Features:

  • Fast cure formula
  • Allows for disassembly
  • Extended shelf life
  • Non-sagging

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
Tensile Strength at Break 2.07 MPa300 psi50% RH
Elongation at Break 750 %750 %50% RH
Shear Strength 0.152 MPa22.0 psiOverlap, Acrylic, 50% RH
 0.262 MPa38.0 psiOverlap, Aluminum, 50% RH
 0.427 MPa62.0 psiOverlap, Glass, 50% RH
 0.441 MPa64.0 psiOverlap, Polypropylene, 50% RH
 0.889 MPa129 psiOverlap, Teak, 50% RH
 0.931 MPa135 psiOverlap, Fir, 50% RH
 0.938 MPa136 psiOverlap, ABS, 50% RH
 0.951 MPa138 psiOverlap, Stainless Steel, 50% RH
 1.20 MPa174 psiOverlap, Polycarbonate, 50% RH
 1.28 MPa185 psiOverlap, Pine, 50% RH
 1.34 MPa195 psiOverlap, Oak, 50% RH
 1.50 MPa218 psiOverlap, Maple, 50% RH
 1.68 MPa244 psiOverlap, Gelcoat, 50% RH
 1.78 MPa258 psiOverlap, Fiberglass, 50% RH
 1.79 MPa260 psiOverlap, Mahogany, 50% RH
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 88.0 °C190 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 16.0 - 26.0 °C
12.0 Month
@Temperature 60.8 - 78.8 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP-100 Epoxy Adhesive
3M Scotchkote™ HTX 517 Epoxy HT Lining
Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
Overview of materials for High Density Polyethylene (HDPE), Extruded
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray

PMM33152 / 167899

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.