MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Silastic® LSR 9451-1000P
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes:

Former Dow Corning brand.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/cc
@Temperature 25.0 °C
Solids Content 100 %
Viscosity 86000 cPdynamic
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 29
Tensile Strength, Ultimate 142 psi
Elongation at Break 311 %
 
Processing PropertiesOriginal ValueComments
Pot Life 1440 min
Shelf Life 18.0 Month
 
Descriptive Properties
Appearancetranslucent
Mix Ratio (X:1)10Base to Catalyst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vicone High Performance Rubber VicoSeal™ 003R-BK Rubber Vulcanized to Steel
Parker Chomerics CHO-SEAL® E6434E Conductive EPDM Elastomer
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
E-Polymers EFLEX® V1050 EPDM/TPV
Dow Nordel® NDR 3722P EPDM Hydrocarbon Rubber

PDOWCO550 / 106251

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.