MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-SEAL® E6434E Conductive EPDM Elastomer  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Extruded Conductive EPDM Elastomer. This is an extruded conductive elastomer engineered for resistance to harsh chemicals, specifically those associated with decontaminates for military Nuclear, Biological, and Chemical requirements. These gaskets are available in continuous extruded profiles for EMI gasketing of large areas.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity >= 2.00 g/cc>= 2.00 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 73 - 8773 - 87ASTM D2240
Elongation at Break >= 100 %>= 100 %ASTM D412
Tear Strength 12.26 kN/m69.96 pli
Compression Set 40 %
@Temperature 100 °C,
Time 252000 sec
40 %
@Temperature 212 °F,
Time 70.0 hour
D395
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.050 ohm-cm0.050 ohm-cmas supplied (without psa); MIL-G-83528
Shielding Effectiveness >= 90 dB>= 90 dB20MHz - 10GHz; MIL-G-83528
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -45.0 °C-49.0 °F
 
Descriptive Properties
BinderEPDM
EMP Survivability kA / in, min0.05
FillerAg/Ni
GradeMilitary-Aerospace
Heat Aging ohm-cm max0.05
Vibration Resistance, After, ohm-cm max0.05
Vibration Resistance, During, ohm-cm max0.05

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ethylene Propylene Rubber (EPM, EPDM)
Dow Nordel® NDR 3722P EPDM Hydrocarbon Rubber
Vicone High Performance Rubber VicoSeal™ 07EK-BK High Performance EPDM Rubber
ATG s.r.l. EPDM Ethylene-Propylene Terpolymer
Armacell Monarch® F-03091 (Black) Pure EPDM Foam

PCHOME137 / 28359

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.