MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Telcar® TL-3260R Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Telcar TL-3260R is a general purpose thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Telcar TL-3260R is a high hardness, high hardness, high density grade that is RoHS compliant. This grade is UL 94V-0 rated and is suitable for both injection molding and extrusion.

Features: Bondability; Chemical Resistant; Filled; Flame Retardant; Good Adhesion; Good Processability; Good Tear Strength; Good Toughness; Halogenated; High Density; High Hardness; High Specific Gravity

Uses: Building Wire Insulation; Fiber Optic Cable Jacketing; General Purpose; Industrial Applications; Rubber Replacement; Wire & Cable Applications; Wire Jacketing

Form: Pellets

Processing Method: Injection Molding; Extrusion

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Viscosity 701 cP
@Temperature 200 °C
701 cP
@Temperature 392 °F
Apparent, 206 sec^-1; ASTM D3835
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 51515 seconds; ASTM D2240
 56561 second; ASTM D2240
 58.3
@Treatment Temp. 230 °C,
Time 3.629e+6 sec
58.3
@Treatment Temp. 446 °F,
Time 1008 hour
ISO 188
Tensile Strength at Break 10.7 MPa1550 psiFlow; ASTM D412
 11.0 MPa1600 psiAcross Flow; ASTM D412
 10.7 MPa
@Treatment Temp. 230 °C,
Time 3.629e+6 sec
1550 psi
@Treatment Temp. 446 °F,
Time 1008 hour
Across Flow, in Air; ISO 188
 11.0 MPa
@Treatment Temp. 257 °C,
Time 605000 sec
1600 psi
@Treatment Temp. 495 °F,
Time 168 hour
Flow, in Air; ISO 188
 11.0 MPa
@Treatment Temp. 230 °C,
Time 3.629e+6 sec
1600 psi
@Treatment Temp. 446 °F,
Time 1008 hour
Across Flow, in Air; ISO 188
 11.3 MPa
@Treatment Temp. 257 °C,
Time 605000 sec
1640 psi
@Treatment Temp. 495 °F,
Time 168 hour
Flow, in Air; ISO 188
Tensile Stress at Strain  7.17 MPa
@Strain 100 %
1040 psi
@Strain 100 %
Across Flow; ASTM D412
 10.7 MPa
@Strain 100 %
1550 psi
@Strain 100 %
Flow; ASTM D412
Elongation at Break 240 %240 %Flow; ASTM D412
 660 %660 %Across Flow; ASTM D412
 226 %
@Treatment Temp. 257 °C,
Time 605000 sec
226 %
@Treatment Temp. 495 °F,
Time 168 hour
Flow, in Air; ISO 188
 239 %
@Treatment Temp. 230 °C,
Time 3.629e+6 sec
239 %
@Treatment Temp. 446 °F,
Time 1008 hour
Across Flow, in Air; ISO 188
 658 %
@Treatment Temp. 230 °C,
Time 3.629e+6 sec
658 %
@Treatment Temp. 446 °F,
Time 1008 hour
Across Flow, in Air; ISO 188
 679 %
@Treatment Temp. 257 °C,
Time 605000 sec
679 %
@Treatment Temp. 495 °F,
Time 168 hour
Flow, in Air; ISO 188
Tear Strength 80.1 kN/m457 pliAcross Flow; ASTM D624
Compression Set  47 %
@Temperature 22.8 °C,
Time 79200 sec
47 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395
 86 %
@Temperature 70.0 °C,
Time 79200 sec
86 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 97 %
@Temperature 90.0 °C,
Time 252000 sec
97 %
@Temperature 194 °F,
Time 70.0 hour
ASTM D395
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  2.32
@Frequency 1000 Hz
2.32
@Frequency 1000 Hz
ASTM D150
 2.33
@Frequency 1e+6 Hz
2.33
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 28.3 kV/mm720 kV/inASTM D149
Dissipation Factor  0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
ASTM D150
 0.00040
@Frequency 1000 Hz
0.00040
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -68.0 °C<= -90.4 °FASTM D746
Flammability, UL94 V-0
@Thickness 1.52 mm
V-0
@Thickness 0.0600 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 193 °C340 - 380 °F
Middle Barrel Temperature 177 - 199 °C350 - 390 °F
Front Barrel Temperature 182 - 204 °C360 - 400 °F
Nozzle Temperature 188 - 210 °C370 - 410 °F
Zone 1 166 - 188 °C330 - 370 °F
Zone 2 171 - 193 °C340 - 380 °F
Zone 3 177 - 199 °C350 - 390 °F
Zone 4 350 - 390 °C662 - 734 °F
Zone 5 182 - 204 °C360 - 400 °F
Die Temperature 190 - 210 °C374 - 410 °F
Melt Temperature 188 - 210 °C370 - 410 °FProcessing Temperature
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex UNIPRENE® 7010-64 Thermoplastic Elastomer
Teknor Apex UNIPRENE® 2023 Thermoplastic Elastomer
Teknor Apex UNIPRENE® 2021 Thermoplastic Elastomer
Teknor Apex UNIPRENE® 2005 Thermoplastic Elastomer

PTEKNP494 / 129575

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.