Notes: Telcar TL-3260R is a general purpose thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Telcar TL-3260R is a high hardness, high hardness, high density grade that is RoHS compliant. This grade is UL 94V-0 rated and is suitable for both injection molding and extrusion. Features: Bondability; Chemical Resistant; Filled; Flame Retardant; Good Adhesion; Good Processability; Good Tear Strength; Good Toughness; Halogenated; High Density; High Hardness; High Specific Gravity Uses: Building Wire Insulation; Fiber Optic Cable Jacketing; General Purpose; Industrial Applications; Rubber Replacement; Wire & Cable Applications; Wire Jacketing Form: Pellets Processing Method: Injection Molding; Extrusion Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpm Information Provided by Teknor Apex |