MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay FM® 50 Foam Adhesive
Categories: Polymer; Adhesive

Material Notes: Description: FM® 50 is a non-MDA-based polyimide foam material intended for core-splicing applications requiring 500 – 600°F (260 – 316°C) service. FM 50 may be cured in place with either a free or restrained foaming process. It contains no metallic fillers.

Features & Benefits:

  • 600°F (316°C) service temperature
  • 350°F (177°C) processing temperature
  • Contains no MDA
  • Radar transparent
  • Superior thermal oxidative stability
  • Co-curable with Avimid® N and other polyimide composite materials
  • Condensation-type polyimide
Applications:
  • High temperature core splice and edge sealing applications

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.057 g/ccUncured
Volatiles 25 %
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 95.0 psiTube
 1200 psiLap
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 316 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay FM® 57 Polyimide Film Adhesive
Henkel Hysol MA 560 Core Splice Adhesive
3M Fastbond™ 100 Neutral Foam Adhesive
Saint-Gobain COHRlastic® 512AF Silicone Foam/Acrylic Adhesive Pressure Sensitive Tape
Solvay FM® 73 Epoxy Film Adhesive

PCYTED042 / 180344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.