MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Polyram RamShine PV527 Acrylonitrile Butadiene Styrene, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Flame retardant ABS for injection molding applications.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inISO 2577
Melt Flow 55 - 60 g/10 min
@Load 10.0 kg,
Temperature 220 °C
55 - 60 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psiISO 527
Elongation at Break 4.0 %4.0 %ISO 527
Tensile Modulus 2.30 GPa334 ksiISO 527
Flexural Strength 75.0 MPa10900 psiISO 178
Flexural Modulus 2.50 GPa363 ksiISO 178
Izod Impact, Notched (ISO) 9.50 kJ/m²4.52 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C187 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C174 °FISO 75
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Glow Wire Ignition Temperature 700 °C1290 °FIEC 60695
Glow Wire Flammability Index 960 °C1760 °FIEC 60695

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram RamShine PV504WT/GR Acrylonitrile Butadiene Styrene, Flame Retardant
Westlake Plastics Absylux® FR Acrylonitrile-Butadiene-Styrene Flame Retardant
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Nylon 46, Unreinforced

PPOLYR955 / 126752

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.