MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Telcar® TL-2895E X Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Telcar TL-2895E X is a general purpose thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. It is a medium hardness, low density, sunlight resistant grade that is RoHS compliant. This grade is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Ablation Resistant; Filled; General Purpose; Halogen Free; High Elasticity; High Elongation; High Tensile Strength; Light Stabilized; Low Density; Medium Hardness; Low Flow; Low Specific Gravity; Sunlight Resistant; UV Absorbing

Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing

RoHS Compliant:RoHS

Form: Pellets

Processing Method: Injection Molding; Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccASTM D792
Melt Flow 5.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
@Time 5.00 sec
ASTM D2240
 85
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 1470 psiFlow, Die C, 20 in/min; ASTM D412
 2630 psiAcross Flow, Die C, 20 in/min; ASTM D412
Tensile Stress at Strain 592 psi
@Strain 100 %
Across Flow, Die C, 20 in/min; ASTM D412
 753 psi
@Strain 300 %
Across Flow, Die C, 20 in/min; ASTM D412
 843 psi
@Strain 100 %
Flow, Die C, 20 in/min; ASTM D412
 1040 psi
@Strain 300 %
Flow, Die C, 20 in/min; ASTM D412
Elongation at Break 580 %Flow, Die C, 20 in/min; ASTM D412
 810 %Across Flow, Die C, 20 in/min; ASTM D412
Tear Strength 317 pliFlow, Die C, 20 in/min; ASTM D624
 335 pliAcross Flow, Die C, 20 in/min; ASTM D624
Compression Set 23 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 79 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 430 - 445 °FInjection, Melt
Rear Barrel Temperature 390 - 420 °FInjection
Middle Barrel Temperature 415 - 430 °FInjection
Front Barrel Temperature 430 - 440 °FInjection
Nozzle Temperature 430 - 445 °FInjection
Zone 1 380 - 410 °FExtrusion
Zone 2 390 - 420 °FExtrusion
Zone 3 415 - 430 °FExtrusion
Zone 5 430 - 440 °FExtrusion
Die Temperature 430 - 445 °FExtrusion
Mold Temperature 77.0 - 150 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 50.0 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1663 / 238154

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.