Telcar TL-2895E X is a general purpose thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. It is a medium hardness, low density, sunlight resistant grade that is RoHS compliant. This grade is suitable for injection molding and extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Ablation Resistant; Filled; General Purpose; Halogen Free; High Elasticity; High Elongation; High Tensile Strength; Light Stabilized; Low Density; Medium Hardness; Low Flow; Low Specific Gravity; Sunlight Resistant; UV Absorbing Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing RoHS Compliant:RoHS Form: Pellets Processing Method: Injection Molding; Extrusion Preliminary data. Information provided by Teknor Apex |