MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eurotec® Tecotek® PC50 GR10 GR053 FA20 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 9002
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccISO 1183
Moisture Absorption 0.200 %
@Temperature 23.0 °C
50% RH; ISO 960
Linear Mold Shrinkage, Flow 0.0050 cm/cmEurotec
Linear Mold Shrinkage, Transverse 0.0050 cm/cmEurotec
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527
Elongation at Break 4.0 %ISO 527
Tensile Modulus 4000 MPaISO 527
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Comparative Tracking Index 175 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 140 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 130 °CISO 75
Vicat Softening Point 140 °C
@Load 5.10 kg
ISO 306
Flammability, UL94 V-0
@Thickness 0.750 mm
 V-0
@Thickness 1.60 mm
Glow Wire Ignition Temperature 900 °C
@Thickness 2.00 mm
IEC 60695
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 - 290 °C
Feed Temperature 60.0 - 80.0 °CThroat
Mold Temperature 80.0 - 100 °C
Drying Temperature 120 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.10 %ISO 960
Hold Pressure 60.0 - 120 MPa
 
Descriptive Properties
Back PressureLow
Injection SpeedMedium - Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural
Cheng Yu Plastic ML3410 PC, 10% Glass Fiber
Mocom (ALBIS) ALTECH® PC ECO 2010/121 GF10 IM UV PC, 10% Glass Fiber Reinforced
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black
RTP Company EMI 331 G FR Polycarbonate (PC), 10% Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant

PEUROS165 / 147155

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.