MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cheng Yu Plastic ML3410 PC, 10% Glass Fiber
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm0.0060 - 0.012 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9090ASTM D785
Tensile Strength, Yield 83.4 MPa12100 psiASTM D638
Flexural Yield Strength 127 MPa18500 psiASTM D790
Izod Impact, Notched 0.981 J/cm1.84 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C295 °FASTM D648
Flammability, UL94 V-2V-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black
Eurotec® Tecotek® PC50 GR10 GR053 FA20 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 9002
Edinburg Plastics CGG625 PC, 10% Glass Filled
Lavergne VYTEEN PCGF10BK PC 10% Glass Reinforced

PLCH069 / 79217

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.