MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® HTplus M3033 PA10T/X, GF30  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: VESTAMID HTplus M3033 is a PA 10T-based, black colored, glass-fiber reinforced (30%), heat-stabilized copolyamide. PA 10T is a poly-condensation product of 1,10-decamethylene diamine (10) and terephthalic acid (T). As 1,10-decamethylene diamine is derived from castor oil plants, VESTAMID HTplus M3033 is partially natural resourced and thus bio-based. Compared to PA 6T-based resins VESTAMID HTplus M3033 has a broader processing window as well as a reduced tendency to absorb water. Therefore the material exhibits less variation in mechanical properties and dimensional changes with humidity. This resin is especially suited for manufacturing parts subjected to high temperature.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 169 MPaISO 527-1
Elongation at Break 2.4 %ISO 527-1
Tensile Modulus 9400 MPaISO 527-1
Charpy Impact Unnotched 52.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 56.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 7.50 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 8.60 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 285 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 284 °CISO 75-1
Deflection Temperature at 1.8 MPa (264 psi) 263 °CISO 75-1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAMID® HTplus F1001 Polyphthalamide
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30
Evonik VESTAMID® HTplus C2505 PA10T/X
Evonik VESTAMID® HTplus M1031 Polyphthalamide

PEVONIL247 / 196451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.