MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Evonik VESTAMID® HTplus C2505 PA10T/X  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: VESTAMID HTplus C2505 is a freeze ground powder based on a PA10T-copolyamide. PA10T is a polycondensation product of 1,10-decamethylene diamine (10) and terephthalic acid (T). As 1,10-decamethylene diamine is derived from castor oil plants, VESTAMID HTplus C2505 is partially natural resourced and thus bio-based. VESTAMID HTplus C2505 exhibits a particle size up to 63 µm. This powder resin is especially suited for manufacturing parts subjected to high temperature.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Particle Size 20 µm20 µmd10
 50 µm50 µmd50
 80 µm80 µmd80
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.0 MPa8990 psiISO 527-1
Elongation at Break >= 100 %>= 100 %ISO 527-1
Tensile Modulus 2.10 GPa305 ksiISO 527-1
Charpy Impact Unnotched  >= 10.0 J/cm²
@Temperature -30.0 °C
>= 47.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 265 °C509 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FISO 75-1
Deflection Temperature at 1.8 MPa (264 psi) 124 °C255 °FISO 75-1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTAMID® HTplus LDS3031 PA10T/X, GF10
Evonik VESTAMID® HTplus F1001 Polyphthalamide
Evonik VESTAMID® HTplus F2001 PA10T/X
Evonik VESTAMID® HTplus M1900 PA6T/X
Evonik VESTAMID® HTplus M1031 Polyphthalamide

PEVONIL236 / 196440

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.