MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TPC Group TPC 5230 Highly Reactive Grade Polyisobutylene
Categories: Polymer

Material Notes: Characteristics: TPC 5230 is colorless (water white), has very low moisture transition rates, is non-corrosive, can be used for emulsions and is hydrophobic with a molecular weight range of 2100 – 2500. TPC 5230 is a highly reactive polyisobutylene (HR-PIB) grade, which means that greater than 80% of its double bonds are in the terminal position of the molecule (alpha).

Applications: TPC 5230 can be used for a variety of applications such as: fuel and lubricant oil additives, emulsifiers, viscosity modifiers, pour point depressants, corrosion inhibitors, tackifiers, PIBSA reactions, polyethylene stretch/cling films, emulsions, asphalt/bitumen and various adhesives and sealants .

General: HR-PIB is especially valued in the fuel and lubricant market as it delivers improved end product performance to the consumer and better manufacturing economics for the additive supplier. Processing with HR-PIB also produces less char during manufacture and the derivative products are used to improve funal lubricant and fuel performance. TPC Group offers the broadest portfolio of PIB products to the market and is a major supplier to many different markets, including fuels and lubricants, caulks, sealants, adhesives, packaging, greases and emulifiers.

Packaging: TPC 5230 is typically sold in railcar quantities.

Information provided by TPC Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 - 0.930 g/cc
@Temperature 15.6 °C
ASTM D4052
Viscosity Measurement 237Index; ASTM D2270
Kinematic Viscosity 1400 - 1800 cStASTM D445
 1615 cSt
@Temperature 100 °C
ASTM D445
 7373 cSt
@Temperature 70.0 °C
ASTM D445
 51045 cSt
@Temperature 40.0 °C
ASTM D445
 265000 cSt
@Temperature 20.0 °C
ASTM D445
Molecular Weight 2100 - 2500 g/mol
Evaporation Loss 0.10 %
@Temperature 99.0 °C,
Time 36000 sec
ASTM D972
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.10[mg KOH/g]; ASTM D974
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 50000 VASTM D877
Dissipation Factor 0.000080
@Temperature 100 °C
ASTM BS5737
 
Thermal PropertiesOriginal ValueComments
Pour Point 12.0 °CASTM D97
Flash Point >= 210 °CCOC; ASTM D92
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5055ASTM D1218
Haze <= 4.0 %Photometric; ASTM D6181
 
Descriptive Properties
AppearanceClear and Bright
Bromine Number6.9 g Br2/100gASTM 1159
Content<1 ppmChlorine, ASTM D4327
 <1 ppmSulfur, ASTM D2622
 <1 ppmAromatics
 >80%Alpha Vinylidene
 25 ppmWater, ASTM D1533
Power Factor8E-05100°C, ASTM D924
Saponification Number<1 mg KOH/gASTM D94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTPCG002 / 320504

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.