MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Gold Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Gold Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.18 - 19.9 g/ccAverage value: 15.2 g/cc Grade Count:141
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 25.0 - 169Average value: 88.2 Grade Count:6
Hardness, Knoop 131 - 2300Average value: 694 Grade Count:4
Hardness, Rockwell A 40.0 - 53.0Average value: 45.7 Grade Count:3
Hardness, Rockwell B 64.0 - 86.0Average value: 74.3 Grade Count:3
Hardness, Rockwell 15T 61.0 - 91.0Average value: 77.2 Grade Count:6
Hardness, Vickers 25.0 - 1060Average value: 177 Grade Count:67
Tensile Strength, Ultimate 120 - 1900 MPaAverage value: 449 MPa Grade Count:83
Tensile Strength, Yield 80.0 - 907 MPaAverage value: 457 MPa Grade Count:56
Elongation at Break 1.20 - 56.5 %Average value: 20.6 % Grade Count:84
Modulus of Elasticity 59.1 - 279 GPaAverage value: 104 GPa Grade Count:40
Compressive Yield Strength 128 - 758 MPaAverage value: 514 MPa Grade Count:4
Poissons Ratio 0.210 - 0.420Average value: 0.378 Grade Count:6
Shear Modulus 26.2 - 28.1 GPaAverage value: 27.4 GPa Grade Count:4
Shear Strength 185 - 276 MPaAverage value: 227 MPa Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000220 - 0.0000620 ohm-cmAverage value: 0.0000175 ohm-cm Grade Count:57
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.90 - 19.5 µm/m-°CAverage value: 15.1 µm/m-°C Grade Count:61
Specific Heat Capacity 0.128 - 0.150 J/g-°CAverage value: 0.133 J/g-°C Grade Count:7
Thermal Conductivity 21.0 - 301 W/m-KAverage value: 64.7 W/m-K Grade Count:33
Melting Point 280 - 1880 °CAverage value: 915 °C Grade Count:179
Solidus 280 - 1290 °CAverage value: 869 °C Grade Count:165
Liquidus 280 - 1450 °CAverage value: 927 °C Grade Count:165
 
Optical PropertiesOriginal ValueComments
Reflection Coefficient, Visible (0-1) 0.270 - 0.850Average value: 0.695 Grade Count:4
 
Processing PropertiesOriginal ValueComments
Processing Temperature 315 - 1230 °CAverage value: 746 °C Grade Count:73
Casting Temperature 950 - 1430 °CAverage value: 1160 °C Grade Count:50
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd 0.00100 %Average value: 0.00100 % Grade Count:8
Carbon, C 0.00500 - 0.0100 %Average value: 0.00714 % Grade Count:7
Cobalt, Co 0.0600 - 0.800 %Average value: 0.520 % Grade Count:3
Copper, Cu 0.000 - 97.0 %Average value: 21.1 % Grade Count:87
Germanium, Ge 12.0 %Average value: 12.0 % Grade Count:5
Gold, Au 3.00 - 100 %Average value: 69.2 % Grade Count:190
Indium, In 0.200 - 25.0 %Average value: 4.73 % Grade Count:31
Iridium, Ir 0.100 - 0.300 %Average value: 0.122 % Grade Count:27
Iron, Fe 0.200 - 1.00 %Average value: 0.400 % Grade Count:4
Lead, Pb 0.00200 %Average value: 0.00200 % Grade Count:8
Manganese, Mn 6.80 - 16.0 %Average value: 10.2 % Grade Count:4
Nickel, Ni 1.15 - 36.5 %Average value: 18.0 % Grade Count:40
Palladium, Pd 1.00 - 76.0 %Average value: 12.7 % Grade Count:54
Phosphorus, P 0.00200 - 0.200 %Average value: 0.0268 % Grade Count:8
Platinum, Pt 0.400 - 30.0 %Average value: 9.15 % Grade Count:39
Rhenium, Re 0.100 %Average value: 0.100 % Grade Count:10
Rhodium, Rh 0.500 - 0.700 %Average value: 0.533 % Grade Count:6
Silicon, Si 2.00 - 3.20 %Average value: 2.78 % Grade Count:3
Silver, Ag 0.500 - 59.2 %Average value: 17.5 % Grade Count:89
Tin, Sn 0.100 - 22.0 %Average value: 14.0 % Grade Count:12
Zinc, Zn 0.00100 - 14.5 %Average value: 5.65 % Grade Count:55

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Grade 2
Titanium Grade 4
Titanium Alloys, General
Titanium Grade 1
Overview of materials for Silver Alloy

M01063 / 81694

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.