MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nexeo® HIVAL® FL19 NT Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Features:
  • BPA Free
  • Food Contact Acceptable
Uses:
  • Closures
  • Household Goods
  • Pails
  • Toys
Agency Ratings: FDA 21 CFR 177.1520

RoHS Compliance: RoHS Compliant

Appearance: Natural Color

Forms: Pellets

Processing Method:

  • Extrusion Coating
  • Injection Molding

Information provided by Nexeo® Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.919 g/cc0.919 g/ccASTM D1505
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545ASTM D2240
Tensile Strength, Yield 9.65 MPa1400 psiASTM D638
Flexural Modulus 0.245 GPa35.5 ksiASTM D790
Izod Impact, Notched 9.08 J/cm
@Temperature -40.0 °C
17.0 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °C104 °FASTM D648
Brittleness Temperature -65.0 °C-85.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 163 °C325 °F
Middle Barrel Temperature 171 °C340 °F
Front Barrel Temperature 177 °C350 °F
Nozzle Temperature 177 °C350 °F
Melt Temperature 177 °C350 °F
Mold Temperature 7.22 - 23.9 °C45.0 - 75.0 °F
Injection Pressure 2.76 - 10.3 MPa400 - 1500 psi
Back Pressure 1.03 - 3.45 MPa150 - 500 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nexeo® HIVAL® 106033 Linear Low Density Polyethylene
Nexeo® HIVAL® 310017 NAT Low Density Polyethylene
Nexeo® HIVAL® 103538 Linear Low Density Polyethylene
Nexeo® HIVAL® 313517 NAT Low Density Polyethylene
LyondellBasell Alathon® H5618 High Density Polyethylene

PNEXEO923 / 197607

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.