MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LD 9519.LN Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: ExxonMobil™ LD 9519.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches. Its flow properties ensure improved processability and uniform dispersion of additives. This resin also offers an outstanding balance of processability and end use performance for injection molding applications.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Caps
  • Closures
  • Compounding
  • Food Packaging Containers
  • Houseware Articles
  • Injection Molding
  • Masterbatch Base Resin

Information provided by ExxonMobil

Key Words: LDPE LD 516.LN
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ExxonMobil method
Melt Flow 9.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
9.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 94
@Time 15.0 sec
94
@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 45
@Time 15.0 sec
45
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 8.27 MPa1200 psiASTM D638
Tensile Strength, Yield 11.7 MPa1700 psiASTM D638
Elongation at Break 87.0 %87.0 %ASTM D638
Elongation at Yield 60 %60 %ASTM D638
Flexural Modulus, 1% Secant 228 MPa33000 psiASTM D790
Dart Drop, Total Energy  16.3 J
@Temperature 22.8 °C
12.0 ft-lb
@Temperature 73.0 °F
ASTM D3763
 19.0 J
@Temperature -20.0 °C
14.0 ft-lb
@Temperature -4.00 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Melting Point 109 °C228 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 85.0 °C185 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LD 40022.LI Low Density Polyethylene Resin
Eastman 1390P Polyethylene
ExxonMobil LD 26019.LN Low Density Polyethylene Resin
ExxonMobil LD 8016.BA Low Density Polyethylene Resin (European Grade)
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin

PEX99235 / 175471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.