Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional stability and the elimination of surface milling operations, ALPLAN® 6061 plates enable to realize significant cost and time savings in machining, when compared to normal rolled plates.Information provided by manufacturer |