MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

RSP Technology RSA-6061 T6 Aluminum Super Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: Ultra fine diamond turned surface finish

Applications:

  • Space mirrors, large mirrors (up to 1 mtr), infrared mirrors, polygon mirrors
Replacing: conventional AA6061, Ni-plating

By replacing conventional 6061 with RSA-6061, surface roughness can be improved by a factor of 4. RSA-6061 can be delivered under official qualifications EN-755 and ASTM-B221.

RSP Technology develops, produces and sells aluminium super alloys with high end properties. By using its own Meltspinning process, ultra fast cooling rates can be reached, converting more than 1 million degrees per second. As a result very fine nanostructured alloys with new functionalities are being developed and produced.

Information provided by RSP Technology BV

Key Words: AA6061
Vendors: RSP Technology – Aluminum as strong as Titanium For more information contact: +31 (0)596 632 300 or visit www.rsp-technology.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.70 g/cc0.0975 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 110110
Tensile Strength, Ultimate 330 MPa47900 psi
Tensile Strength, Yield 300 MPa43500 psi
Elongation at Break 14 %14 %
Tensile Modulus 70.0 GPa10200 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.0 µm/m-°C12.8 µin/in-°F
Thermal Conductivity 160 W/m-K1110 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 98.1 %98.1 %
Copper, Cu 0.30 %0.30 %
Magnesium, Mg 1.1 %1.1 %
Silicon, Si 0.50 %0.50 %
 
Descriptive Properties
Specific Stiffness26GPa/(g/cc)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
Alclad Aluminum 6061-T6, T651
Aluminum 6082-T6
Aluminum 7075-T6; 7075-T651
JIS S45C Steel, Normalized

NRSP20 / 100834

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.