MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
Saint-Gobain Meldin® 6030 PTFE-Filled Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Molded, PTFE Filled

Material Notes: Contains 30% PTFE filler and is a pseudo-thermoplastic material. Lower cost, lower performance analog of Meldin® 2030. Used in high speed self lubricating vanes in air motors.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.53 g/ccASTM D792
Water Absorption 0.90 %
@Temperature 50.0 °C,
Time 173000 sec
ASTM D570
 0.38 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore M 92ASTM D785
Tensile Strength, Yield >= 7000 psiASTM D638
 >= 4000 psi
@Temperature 260 °C
ASTM D638
Elongation at Break 6.0 %ASTM D638
 8.0 %
@Temperature 260 °C
ASTM D638
Tensile Modulus 225000 psiASTM D638
 150000 psi
@Temperature 260 °C
ASTM D638
Flexural Strength 10000 psiASTM D790
 3000 psi
@Temperature 260 °C
ASTM D790
Compressive Strength 30000 psiASTM D695 (Modified)
Izod Impact, Notched 0.600 ft-lb/inASTM D256
Izod Impact, Unnotched 4.00 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.0
@Frequency 10000 Hz
ASTM D150
 3.2
@Frequency 100 Hz
ASTM D150
 3.25
@Frequency 60 Hz
ASTM D150
Dissipation Factor 0.0020
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 27.0 µin/in-°F
Maximum Service Temperature, Air 600 °F
Deflection Temperature at 1.8 MPa (264 psi) 550 °FASTM D648
Minimum Service Temperature, Air -400 °F
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 4299 X 117414 Thermoplastic Polyimide (TPI), Carbon Fiber
Saint-Gobain Meldin® 6001 Polyimide
DuPont Mobility and Materials Vespel® SP-221 DF Polyimide
DuPont Mobility and Materials Vespel® SP-202 Conductive Polyimide
DuPont Mobility and Materials Vespel® SCP-5050 Polyimide

PSTGQZ081y / 192459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.