MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials Vespel® SP-221 DF Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes: Parts from graphite filled PI (polyimide) with Teflon for highly specialized applications against soft metals in "no-lube" conditions.

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 39.0 MPa
@Temperature 23.0 °C
5660 psi
@Temperature 73.4 °F
ASTM D 638
Elongation at Break 3.5 %
@Temperature 23.0 °C
3.5 %
@Temperature 73.4 °F
ASTM D 638
Flexural Strength  31.0 MPa
@Temperature 260 °C
4500 psi
@Temperature 500 °F
ASTM D 790
 55.0 MPa
@Temperature 23.0 °C
7980 psi
@Temperature 73.4 °F
ASTM D 790
Flexural Modulus  2.205 GPa
@Temperature 260 °C
319.8 ksi
@Temperature 500 °F
ASTM D 790
 3.445 GPa
@Temperature 23.0 °C
499.7 ksi
@Temperature 73.4 °F
ASTM D 790
Compressive Strength 112 MPa16200 psiASTM D 695
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 50.0 °C
@Thickness 0.750 mm
122 °F
@Thickness 0.0295 in
UL 746B
UL RTI, Mechanical with Impact 50.0 °C
@Thickness 0.750 mm
122 °F
@Thickness 0.0295 in
UL 746B
UL RTI, Mechanical without Impact 50.0 °C
@Thickness 0.750 mm
122 °F
@Thickness 0.0295 in
UL 746B
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
IEC 60695-11-10
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
UL94
 
Descriptive Properties
Contains Flame RetardantYes
FillerGraphite Powder
Heat StabilizedYes
Polymer FamilyPolyimide
Polymer TypePI
Region AvailableAmericas
 Asia/Pacific
 Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SP-1 ISO Polyimide
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
DuPont Mobility and Materials Vespel® CP-0644 Polyimide
DuPont Mobility and Materials Vespel® SP-22 DF Polyimide
DuPont Mobility and Materials Vespel® SP-2515 Direct Formed (DF) Polyimide Parts

PDTA7759 / 89871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.