MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include:
  • Excellent surface appearance
  • High corrosion and abrasion resistance
  • Excellent toughness
  • High temperature resistance
  • Excellent chemical resistance
  • Electrical isolation and arc resistance
  • High performance
  • Easy processability
  • Fast cycle time
Glass fiber reinforcement imparts high shrinkage resistance and impact resistance to TISESTER products, yielding improvements in thermal features as well. PBT is resistant against solvents, exhibits low shrinkage during shaping, and it is mechanically strong, heat resistant for temperatures up to 150°C, and can be reinforced for flame retardance. Tisester compounds display sufficient resistance against hydrocarbons, alcohols, ethers, acids, and alkali solvents.

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccISO 1183
Moisture Absorption 0.20 %ISO 62
Linear Mold Shrinkage 0.0030 cm/cm
Ash 30 %ISO 3451
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85ISO 868
Tensile Strength at Break 152 MPaISO 527-2
Tensile Strength, Yield 150 MPaISO 527-2
Elongation at Break 2.7 %ISO 527-2
Elongation at Yield 2.5 %ISO 527-2
Modulus of Elasticity 9.50 GPaISO 527-2
Izod Impact, Notched (ISO) 8.50 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 300 VTS EN 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 - 230 °C
Vicat Softening Point 220 °CISO 306
Heat Distortion Temperature 218 °CISO 75-2
Flammability, UL94 V-0
Glow Wire Test 960 °C60695-2-10
 
Processing PropertiesOriginal ValueComments
Feed Temperature 70.0 °C
Rear Barrel Temperature 220 - 250 °CAft-1. Region Temperature
Middle Barrel Temperature 220 - 250 °CMid-2. Region Temperature
Front Barrel Temperature 220 - 250 °CPre-3. Region Temperature
Nozzle Temperature 225 °C
Melt Temperature 220 - 230 °C
Drying Temperature 110 - 120 °CPredrying Temperature
Dry Time 4 - 5 hourPredrying Time
 
Descriptive Properties
Block Temperature80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Tecapeek® XP-96 Compression Molded PEEK
Tisan TISLAMID® 66 20% Glass Fiber Reinforced Nylon 66
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6
Beijing Evergrow Resources MoS2 Filled Nylon

PTIS058 / 79493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.