MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beijing Evergrow Resources MoS2 Filled Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes:

Information provided by Beijing Evergrow Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³GB1033
Water Absorption 6.1 - 6.3 %6.1 - 6.3 %
Moisture Absorption 1.9 - 2.0 %1.9 - 2.0 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 8880 - 88GB3398
Ball Indentation Hardness 148.5 MPa21540 psiGB3398
Tensile Strength at Break 74.1 MPa10700 psiGB/T 1040
Elongation at Yield <= 25 %<= 25 %GB/T 1040
Modulus of Elasticity 3.10 GPa450 ksiGB/T 1040
Flexural Strength 86.9 MPa12600 psiGB9341
Compressive Strength 90.0 - 105 MPa13100 - 15200 psiGB/T 1040
Izod Impact, Notched (ISO) 6.40 kJ/m²3.05 ft-lb/in²GBT1043
Coefficient of Friction 0.1070.107GB3360
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmVolume; GB1410
Arc Resistance 600 sec600 secASTM D112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 75.0 µm/m-°C41.7 µin/in-°FGB1036
Melting Point 230 °C446 °FHG/T2235
Heat Distortion Temperature 145 °C293 °FGB1634

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate
Ensinger Tecapeek® XP-96 Compression Molded PEEK
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK)
Beijing Evergrow Resources Glass Filled Nylon
Tisan TISARBON® Flame Retardant (V0) Polycarbonate

PBEIJ111 / 90180

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.