MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Chemfab® 5 Basic PTFE-Coated Glass
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: Chemfab® Basic Series products are low resin-content, non-porous, PTFE-coated fiberglass fabrics. Applications are spray shields, separator sheets, release sheets and protective barriers from chemicals. Basic is also used in applications where fabric texture is required. Description: Chemfab® Basic is a high-value product with price being the primary feature while still delivering performance. All data based on a 0.004 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 108.33 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Tear Strength Test 3.0Lbs./In. for warp/longitudinal Propagation Tear Strength
 3.5Lbs./In. Propagation Tear Strength in fill/transverse direction
Tear Strength 100 pliTensile Strength (Fill)
 120 pliTensile Strength (Warp)
 
Descriptive Properties
Weight (oz/yd^2)5.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Chemfab® 3 High-Performance PTFE-Coated Glass
Saint-Gobain Chemfab® 10 Basic PTFE-Coated Glass
Saint-Gobain Chemfab® 10 Anti-Static PTFE-Coated Glass
Saint-Gobain Chemfab® 3 Basic PTFE-Coated Glass
Saint-Gobain Chemfab® 13 Anti-Static PTFE-Coated Glass

CSTGQZ135 / 2264

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.