MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Chemfab® 3 High-Performance PTFE-Coated Glass
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat sealing and packaging applications. High-Performance is also a good choice for chemical resistance, food contact, and dielectric requirements. All data based on a 0.0032 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.1276 g/cc0.076857 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tear Strength Test 1.51.5Lbs./In. Propagation Tear Strength in fill/transverse direction
 2.02.0Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 14.0 kN/m80.0 pliTensile Strength (Fill)
 15.8 kN/m90.0 pliTensile Strength (Warp)
 
Descriptive Properties
Weight (oz/yd^2)5.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Chemfab® 5 Basic PTFE-Coated Glass
NeoGraf GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing
Saint-Gobain Chemfab® 10 Basic PTFE-Coated Glass
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
Saint-Gobain Chemfab® 3 Basic PTFE-Coated Glass

CSTGQZ137 / 2266

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.