MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Henkel Loctite® ECCOBOND 931-1T1N1 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: clear

Cure: Heat Cure

Product Benefits:

  • Low viscosity
Application: Die attach

Key Substrates: Glass, Alumina, Ferrite, Aluminum and Steel

LOCTITE ECCOBOND 931-1T1N1 adhesive is designed for medium die attach applications.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 2.00e+14 cP
Brookfield Viscosity 2400 cPUncured, CP51, Speed 5 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88cured 2 hours @ 60ºC
Shear Strength 20.7 MPaLap, Al to Al
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 100 °C
 2.00 hour
@Temperature 60.0 °C
Alternative Cure Schedule
Working Life 4.00 hour
Shelf Life 12.0 Month
@Temperature 5.00 °C
from date of manufacture
 12.0 Month
@Temperature 5.00 °C
from date of manufacture, two-part kits
 12.0 Month
@Temperature -40.0 °C
from date of manufacture, premixed
 
Descriptive Properties
Thixotropic Index2.8Uncured, 0.5/5 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5070 / 255281

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.