MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Henkel Loctite® ECCOBOND 931-1T1N1 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: clear

Cure: Heat Cure

Product Benefits:

  • Low viscosity
Application: Die attach

Key Substrates: Glass, Alumina, Ferrite, Aluminum and Steel

LOCTITE ECCOBOND 931-1T1N1 adhesive is designed for medium die attach applications.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 2.00e+14 cP2.00e+14 cP
Brookfield Viscosity 2400 cP2400 cPUncured, CP51, Speed 5 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888cured 2 hours @ 60ºC
Shear Strength 20.7 MPa3000 psiLap, Al to Al
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 100 °C
2.00 hour
@Temperature 212 °F
 120 min
@Temperature 60.0 °C
2.00 hour
@Temperature 140 °F
Alternative Cure Schedule
Working Life 240 min240 min
Shelf Life  12.0 Month
@Temperature 5.00 °C
12.0 Month
@Temperature 41.0 °F
from date of manufacture
 12.0 Month
@Temperature 5.00 °C
12.0 Month
@Temperature 41.0 °F
from date of manufacture, two-part kits
 12.0 Month
@Temperature -40.0 °C
12.0 Month
@Temperature -40.0 °F
from date of manufacture, premixed
 
Descriptive Properties
Thixotropic Index2.8Uncured, 0.5/5 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOCT5070 / 255281

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.