MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Garlock GYLON® 3510 PTFE Gasketing, Barium Sulfate Filler
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: PTFE with barium sulfate filler.
  • Improved sealing performance over conventional PTFE
  • Unique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheets
  • Excellent bolt torque retention
  • Withstands a wide range of chemicals for extended service life
Media: Strong caustics, Moderate acids, Chlorine, Gases, Water, Steam, Hydrocarbons, Cryogenics and aluminum fluoride

Information provided by Garlock Rubber Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Permeability 0.015Gas Permeability, cc/min; DIN 3535 Part 4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2000 psiacross grain; ASTM F152
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 466 V/mil
@Temperature 121 °C,
Time 10800 sec
0.0625 in. thickness; ASTM D149
 59.0 V/mil
@Thickness 1.59 mm
100% RH for 96 hours; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
@Pressure 8.27 MPa
Continuous
Minimum Service Temperature, Air -450 °F
 
Descriptive Properties
ColorOff-White
Compressibility, %4-10ASTM F36
Creep Relaxation, %11ASTM F38
Sealability ASTM F37B, ml/hr0.04ASTM Fuel A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGARL816 / 157494

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.