MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Plastics Radel® R 5500 Polyphenylsulfone  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Replaced by Thermalux PPSU .

Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress cracking resistance. These properties make Radel R stock shapes attractive for a variety of demanding applications. The standard color of Radel R is off white, but a transparent grade is available.

Radel® is a trade name of Solvay Advanced Polymers. Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccASTM D792
Water Absorption 0.37 %ASTM D570; 24 hrs.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 10100 psiASTM D638
Elongation at Break 60 - 120 %ASTM D638
Elongation at Yield 7.2 %ASTM D638
Tensile Modulus 340000 psiASTM D638
Flexural Yield Strength 13200 psiASTM D790
Flexural Modulus 350000 psiASTM D790
Compressive Yield Strength 14.35 ksiASTM D695
Compressive Modulus 251000 psiASTM D695
Izod Impact, Notched 13.0 ft-lb/inASTM D256
Izod Impact, Unnotched NBASTM D256
Tensile Impact Strength 190 ft-lb/in²ASTM D1822
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+17 ohm-cmASTM D257
Dielectric Constant 3.45
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 360 V/milASTM D149
Dissipation Factor 0.00090
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 2.42 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 417 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 405 °FASTM D648
Flammability, UL94 V-0
@Thickness 0.787 mm
Oxygen Index 38 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Haze 15 %ASTM D1746
Transmission, Visible 50 %ASTM D1746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP Radel R-7625 Polyphenyl Sulfone (PPSU); Flame Retardant
Syensqo (Solvay Specialty Polymers) Radel® R-5900 MR Polyphenylsulfone (PPSU)
Syensqo (Solvay Specialty Polymers) Radel® R-7535 Polyphenylsulfone (PPSU)
Syensqo (Solvay Specialty Polymers) Radel® R-7625 Polyphenylsulfone (PPSU)
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)

PWEST126 / 72758

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.