MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Afton Plastics 450G PEEK Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Afton plastics produces shapes and components from Victrex™ PEEK®, a high-performance thermoplastic that has an extraordinary combination of mechanical, structural and chemical resistance.

Product Benefits: • Wear resistance • Service temperature: -50°F to +500°F • Hydrolysis resistance • Radiation resistance • FDA compliant

Applications: Thrust washers • Pump gears • Compressor valve plates • Electrical connectors • Valve seats and seals • Bearings and bushings.

Information provided by Afton Plastics.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³Crystalline; ISO 1183
Water Absorption at Saturation 0.45 %
@Temperature 23.0 °C
0.45 %
@Temperature 73.4 °F
By immersion; ISO 62-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 84.584.5
Tensile Strength, Yield 98.0 MPa14200 psiISO 527
Elongation at Break 45 %45 %ISO 527
Flexural Strength 125 MPa
@Strain 3.5 %
18100 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 3.80 GPa551 ksiISO 178
Compressive Strength 125 MPa18100 psiISO 604
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Dielectric Constant 3.1
@Frequency 1000 Hz
3.1
@Frequency 1000 Hz
IEC 60250
Dielectric Strength 200 kV/mm5080 kV/in50 µm thickness; IEC 60243-1
Dissipation Factor 0.0040
@Frequency 1e+6 Hz
0.0040
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear  55.0 µm/m-°C
@Temperature <=143 °C
30.6 µin/in-°F
@Temperature <=289 °F
 140 µm/m-°C
@Temperature >=143 °C
77.8 µin/in-°F
@Temperature >=289 °F
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°FISO 22007-4
 0.290 W/m-K2.01 BTU-in/hr-ft²-°FISO 22007-4
Melting Point >= 343 °C>= 649 °FISO 11357
Maximum Service Temperature, Air 250 °C482 °Fcontinuous
Deflection Temperature at 1.8 MPa (264 psi) 152 °C306 °FISO 75-f
Minimum Service Temperature, Air -45.6 °C-50.0 °F
Glass Transition Temp, Tg 143 °C289 °F
Flammability, UL94 V-0V-0
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450G™ General Purpose
Overview of materials for Polyetheretherketone, Unreinforced
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone

PAFTON913 / 232138

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.