MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Aramid Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Victrex is a global leader in high-performance PEEK and PAEK polymers, transforming industries from aerospace to medical devices. For 40 years, our innovative polymer solutions help customers achieve new levels of performance, sustainability, and cost efficiency across applications that millions rely on daily from smartphones to aircraft components. As pioneers in polymer engineering, we're committed to delivering transformational solutions that address global materials challenges. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.31 - 1.50 g/cc0.0473 - 0.0542 lb/in³Average value: 1.37 g/cc Grade Count:12
Linear Mold Shrinkage 0.000500 - 0.0150 cm/cm0.000500 - 0.0150 in/inAverage value: 0.00871 cm/cm Grade Count:12
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 75.0 - 193 MPa10900 - 28000 psiAverage value: 95.0 MPa Grade Count:12
Elongation at Break 1.00 - 6.00 %1.00 - 6.00 %Average value: 3.50 % Grade Count:12
Modulus of Elasticity 4.00 - 20.7 GPa580 - 3000 ksiAverage value: 6.58 GPa Grade Count:12
Flexural Yield Strength 138 - 276 MPa20000 - 40000 psiAverage value: 160 MPa Grade Count:11
Flexural Modulus 4.83 - 22.8 GPa700 - 3300 ksiAverage value: 6.81 GPa Grade Count:11
Izod Impact, Notched 0.267 - 0.641 J/cm0.500 - 1.20 ft-lb/inAverage value: 0.437 J/cm Grade Count:11
Izod Impact, Unnotched 2.67 - 6.41 J/cm5.00 - 12.0 ft-lb/inAverage value: 4.30 J/cm Grade Count:11
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 10000 - 1.00e+16 ohm-cm10000 - 1.00e+16 ohm-cmAverage value: 4.21e+15 ohm-cm Grade Count:6
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 163 - 260 °C325 - 500 °FAverage value: 193 °C Grade Count:8
Flammability, UL94 V-0V-0Grade Count:9
 
Processing PropertiesMetricEnglishComments
Processing Temperature 343 - 388 °C650 - 730 °FAverage value: 366 °C Grade Count:4
Melt Temperature 349 - 399 °C660 - 750 °FAverage value: 374 °C Grade Count:8
Mold Temperature 163 - 218 °C325 - 425 °FAverage value: 190 °C Grade Count:12
Drying Temperature 120 - 150 °C248 - 302 °FAverage value: 147 °C Grade Count:8
Moisture Content 0.100 %0.100 %Average value: 0.100 % Grade Count:7
Dew Point -28.9 °C-20.0 °FAverage value: -28.9 °C Grade Count:7
Injection Pressure 82.7 - 124 MPa12000 - 18000 psiAverage value: 103 MPa Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyetheretherketone, Glass Fiber Filled
Overview of materials for Polyetheretherketone, PTFE Filled
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
Overview of materials for Polyamide-Imide, Molded

O2133 / 77936

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.