MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Fibre Glast 1543 Style 6781 S2-Glass Fabric
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: S-2 Fiberglass has high tensile strength, high heat & chemical resistance, and is dimensionally stable. The resulting composite fabric meets or exceeds military, aerospace, and other relevant specifications. The 6781 style is the most popular aerospace fabric in use today. 1543 is woven with superior S-2 fibers resulting in good strength with a superior look and finish.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 9.70 mil
 
Descriptive Properties
Weave Pattern8-Harness Satin
Weight (oz/sq yd)8.85
Yarn Description, FillSCG 75 1/0
Yarn Description, WarpSCG 75 1/0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexForce™ 6781 Fiber Glass Fabric
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 6781 S2 Glass Fabric
Renegade Materials Corporation RM-3000 Bismaleimide (BMI) 6781 S2 Glass Fabric
Fibre Glast 573 Style 120 E-Glass Fiberglass Fabric
Overview of materials for Epoxy/Carbon Fiber Composite

PFIBRE110 / 104547

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.