MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Renegade Materials Corporation RM-3000 Bismaleimide (BMI) 6781 S2 Glass Fabric
Categories: Polymer; Thermoset; Bismaleimide (BMI); Filled/Reinforced Thermoset

Material Notes: Developed using state-of-the-art formulating technologies, RM-3000 One Part BMI RTM Resin delivers superior hot/wet performance in airframe, missile and propulsion applications at service temperatures up to 400°F. RM-3000 resin delivers improved damage tolerance at higher temperatures vs. industry-standard BMI resins. RM-3000 resin can be injected into a variety of woven and non-crimp fabrics as well as braids and complex engineered preforms. Renegade also offers a similar resin system for Vacuum Assisted RTM (VARTM) processing to support molding of larger parts called RM-3010 and an autoclave prepreg version called RM-3002.

Information provided by Renegade Materials Corporation.

Renegade Materials has been acquired by Teijin.

Key Words: BMI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³Resin
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 4.0 %4.0 %Resin, RT, Dry
 1.4 %
@Temperature 177 °C
1.4 %
@Temperature 350 °F
Wet (140°F/95% RH), 0° Direction; ASTM D6641
 2.3 %
@Temperature 21.1 °C
2.3 %
@Temperature 70.0 °F
Dry, 0° Direction; ASTM D6641
Flexural Strength 145 MPa21000 psiResin
Flexural Modulus 4.27 GPa620 ksiResin
Compressive Strength  352 MPa
@Temperature 177 °C
51000 psi
@Temperature 350 °F
Wet (140°F/95% RH), 0° Direction; ASTM D6641
 710 MPa
@Temperature 21.1 °C
103000 psi
@Temperature 70.0 °F
Dry, 0° Direction; ASTM D6641
Compressive Modulus  28.3 GPa
@Temperature 177 °C
4100 ksi
@Temperature 350 °F
Wet (140°F/95% RH), 0° Direction
 33.8 GPa
@Temperature 21.1 °C
4900 ksi
@Temperature 70.0 °F
Dry, 0° Direction; ASTM D6641
Shear Strength  33.1 MPa
@Temperature 177 °C
4800 psi
@Temperature 350 °F
Wet (140°F/95% RH), In-plane; ASTM D3846
 96.5 MPa
@Temperature 21.1 °C
14000 psi
@Temperature 70.0 °F
Dry, In-plane; ASTM D3846
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Glass Transition Temp, Tg 247 °C477 °FWet, Resin, Storage Modulus
 282 °C540 °FDry, Resin, Storage Modulus

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® F650 Bismaleimide Resin
HOS-Technik Homide 250 Bismaleimide Resin
Evonik Compimide® 353A Bismaleimide
Hexcel® HexPly® F652 Bismaleimide Resin
Renegade Materials Corporation RM-3000 Bismaleimide (BMI) Resin

PRENEG10 / 138465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.