MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Overview of materials for Polyester Thermoplastic Elastomer, Glass Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer, Glass Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer, Glass Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.02 - 2.00 g/cc0.0368 - 0.0723 lb/in³Average value: 1.50 g/cc Grade Count:31
Filler Content 5.00 - 40.0 %5.00 - 40.0 %Average value: 16.9 % Grade Count:8
Water Absorption 0.100 - 1.00 %0.100 - 1.00 %Average value: 0.353 % Grade Count:15
Linear Mold Shrinkage 0.00100 - 0.00900 cm/cm0.00100 - 0.00900 in/inAverage value: 0.00361 cm/cm Grade Count:23
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114 - 116114 - 116Average value: 115 Grade Count:5
Hardness, Shore D 40.0 - 72.040.0 - 72.0Average value: 56.8 Grade Count:8
Tensile Strength, Ultimate 12.4 - 150 MPa1800 - 21800 psiAverage value: 72.8 MPa Grade Count:23
Tensile Strength, Yield 57.2 - 179 MPa8300 - 26000 psiAverage value: 101 MPa Grade Count:14
Elongation at Break 1.80 - 18.0 %1.80 - 18.0 %Average value: 5.97 % Grade Count:22
Elongation at Yield 3.00 - 10.0 %3.00 - 10.0 %Average value: 4.33 % Grade Count:6
Modulus of Elasticity 0.414 - 7.66 GPa60.0 - 1110 ksiAverage value: 3.39 GPa Grade Count:14
Flexural Yield Strength 12.4 - 250 MPa1800 - 36300 psiAverage value: 126 MPa Grade Count:30
 70.0 - 150 MPa
@Temperature 130 - 155 °C
10200 - 21800 psi
@Temperature 266 - 311 °F
Average value: 104 MPa Grade Count:6
Flexural Modulus 0.600 - 13.8 GPa87.0 - 2000 ksiAverage value: 4.76 GPa Grade Count:22
Compressive Yield Strength 11.0 - 400 MPa1600 - 58000 psiAverage value: 195 MPa Grade Count:11
Izod Impact, Notched 0.427 - 4.81 J/cm0.800 - 9.00 ft-lb/inAverage value: 1.88 J/cm Grade Count:22
Izod Impact, Unnotched 5.34 J/cm - NB10.0 ft-lb/in - NBAverage value: 8.80 J/cm Grade Count:13
Izod Impact, Notched (ISO) 8.00 - 33.3 kJ/m²3.81 - 15.8 ft-lb/in²Average value: 17.8 kJ/m² Grade Count:4
 7.00 - 13.0 kJ/m²
@Temperature -40.0 - -40.0 °C
3.33 - 6.19 ft-lb/in²
@Temperature -40.0 - -40.0 °F
Average value: 10.3 kJ/m² Grade Count:3
Charpy Impact, Notched 3.00 - 12.0 J/cm²14.3 - 57.1 ft-lb/in²Average value: 5.29 J/cm² Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 - 1.00e+16 ohm-cm1.00e+13 - 1.00e+16 ohm-cmAverage value: 5.25e+15 ohm-cm Grade Count:4
Insulation Resistance 5.00e+8 - 1.00e+11 ohm5.00e+8 - 1.00e+11 ohmAverage value: 2.79e+10 ohm Grade Count:8
Dielectric Constant 4.72 - 4.934.72 - 4.93Average value: 4.80 Grade Count:3
Dielectric Strength 9.00 - 19.7 kV/mm229 - 500 kV/inAverage value: 13.3 kV/mm Grade Count:12
Dielectric Breakdown 40000 - 80000 V40000 - 80000 VAverage value: 62500 V Grade Count:8
Dissipation Factor 0.0240 - 0.07800.0240 - 0.0780Average value: 0.0477 Grade Count:3
Arc Resistance 60.0 - 130 sec60.0 - 130 secAverage value: 104 sec Grade Count:3
Comparative Tracking Index 500 - 600 V500 - 600 VAverage value: 550 V Grade Count:8
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 198 µm/m-°C11.1 - 110 µin/in-°FAverage value: 47.3 µm/m-°C Grade Count:11
Maximum Service Temperature, Air 155 - 210 °C311 - 410 °FAverage value: 168 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 199 °C176 - 390 °FAverage value: 138 °C Grade Count:9
Deflection Temperature at 1.8 MPa (264 psi) 48.9 - 226 °C120 - 439 °FAverage value: 143 °C Grade Count:20
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:12
 
Optical PropertiesMetricEnglishComments
Haze 48.0 - 99.0 %48.0 - 99.0 %Average value: 81.6 % Grade Count:5
Transmission, Visible 70.0 - 84.0 %70.0 - 84.0 %Average value: 77.2 % Grade Count:5
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 232 °C380 - 450 °FAverage value: 213 °C Grade Count:8
Nozzle Temperature 277 - 291 °C531 - 556 °FAverage value: 284 °C Grade Count:8
Melt Temperature 216 - 288 °C421 - 550 °FAverage value: 273 °C Grade Count:15
Mold Temperature 21.1 - 116 °C70.0 - 241 °FAverage value: 60.1 °C Grade Count:23
Drying Temperature 71.0 - 120 °C160 - 248 °FAverage value: 102 °C Grade Count:15
Moisture Content 0.0200 - 0.100 %0.0200 - 0.100 %Average value: 0.0360 % Grade Count:10
Dew Point -40.0 °C-40.0 °FAverage value: -40.0 °C Grade Count:8
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiAverage value: 86.2 MPa Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
Overview of materials for Polyester Thermoplastic Elastomer
Overview of materials for Thermoset Polyester Glass Filled BMC
Advanced Elastomer Systems Santoprene® 101-64 W175 Thermoplastic Rubber
Overview of materials for Thermoset Polyester Glass SMC

O5411 / 78500

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.