MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Adell BS-10 Nylon 6, General Purpose
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Data provided by Adell Plastics, Inc.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM D792
Water Absorption 1.8 %1.8 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0125 cm/cm0.0125 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7878ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Ultimate 75.8 MPa11000 psiASTM D638
Elongation at Break 60 %60 %ASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
Flexural Modulus 2.70 GPa392 ksiASTM D790
Compressive Yield Strength 62.0 MPa8990 psiASTM D695
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 182 °C360 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C147 °FASTM D648
Flammability, UL94 V-2V-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Manifattura Cattaneo PA 6 Nylon
BASF Capron® 1202CQ Nylon 6 (Dry)
Adell BS-30 Nylon 6, General Purpose

PDEL04 / 29565

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.