MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carbon-Core Plastic Honeycomb
Categories: Other Engineering Material

Material Notes: The mechanical properties of Carbon-Core Honeycomb are controlled by the following specifications: 1) physical properties of the thermoplastic; 2) cell diameter; 3) wall gauge (thickness of the cell wall); 4) core thickness; and 5) facings applied to the core. Altering one or more of these specifications will produce different performance characteristics. Carbon-Core honeycombs can be engineered to be a specific weight, absorb a specific load, rebound at a specified rate and possess the flexibility or stiffness required by the end application.

Information provided by Carbon-Core

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0801 g/cc0.00289 lb/in³
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.896 MPa130 psiISO 844
Compressive Strength 1.90 MPa275 psiISO 844
Compressive Modulus 0.079179 GPa11.484 ksiISO 844
Shear Modulus 0.01520 GPa2.205 ksiISO 1922
Shear Strength 0.586 MPa85.0 psiISO 1922
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0300 W/m-K0.208 BTU-in/hr-ft²-°F
 
Descriptive Properties
Dimensional Stability-40-110°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NMG ProCell® PC48 PVC Foam Core
3M 4718 Single-Coated Foam Tape
Röhm ACRYLITE® 8 mm Resist High Impact Acrylic Double-Skin Sheet
ERG Aerospace Duocel® Aluminum Metal Foam
Carbon-Core CarbonFoam 100 PET

PCARBC029 / 190848

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.