MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carbon-Core CarbonFoam 100 PET
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Special Features:
  • Thermoformable
  • Great fatigue resistance
  • Good chemical resistance
  • No toxic or corrosive emissions when burned

    Information provided by Carbon-Core

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.101 g/cc0.00365 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 2.10 MPa305 psiASTM D1623
Tensile Modulus 0.1071 GPa15.53 ksiASTM D1623
Compressive Strength 1.86 MPa270 psiISO 844
Compressive Modulus 0.084178 GPa12.209 ksiISO 844
Shear Modulus 0.02790 GPa4.046 ksiASTM C273
Shear Strength 1.19 MPa173 psiASTM C273
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0150 W/m-K0.104 BTU-in/hr-ft²-°FISO 12667
 
Descriptive Properties
Closed Cell RateISO 4590
Dimensional Stability175°C
Fire ResistanceFMVSS 302DIN 4102 M1F1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET
Celanese Rynite® 408 NC010 PET
DIAB Divinycell® PX 60 Sandwich Core Material

PCARBC003 / 190822

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.