MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, High Strength 12k Carbon Balanced Fabric 600 g/m2
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 60.0 %Fiber Volume
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 900 MPa
Tensile Modulus 65.0 GPa
Flexural Yield Strength 950 MPa
Flexural Modulus 65.0 GPa
Compressive Yield Strength 600 MPa
Shear Strength 70.0 MPa0º, Short Beam
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow E-glass/Epoxy Composite
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape Not Supported 150 g/m2
Hexcel® HexPly® M10E Epoxy Resin, Carbon Tapes
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber

PHEXC171 / 98642

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.