MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³Resin Density
 1.78 g/cc0.0643 lb/in³Fiber Density
Filler Content 55.0 %55.0 %Fiber Volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 850 MPa123000 psi90º, RT, Dry; EN2561
 750 MPa
@Temperature 135 °C
109000 psi
@Temperature 275 °F
90º, Wet; EN2561
Tensile Modulus 62.8 GPa9110 ksi90º, RT, Dry; EN2561
 60.0 GPa
@Temperature 135 °C
8700 ksi
@Temperature 275 °F
90º, Wet; EN2561
Compressive Yield Strength 730 MPa106000 psi90º, RT, Dry; EN2850 Type B
 530 MPa
@Temperature 135 °C
76900 psi
@Temperature 275 °F
90º, Wet; EN2850 Type B
Shear Strength 65.0 MPa9430 psi0º, ILSS Short Beam, RT, Dry; EN2563
 35.0 MPa
@Temperature 135 °C
5080 psi
@Temperature 275 °F
0º, ILSS Short Beam, Wet; EN2563
 49.0 MPa
@Temperature 120 °C
7110 psi
@Temperature 248 °F
0º, ILSS Short Beam, Dry; EN2563
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 - 130 °C248 - 266 °FEpoxy Matrix Limit
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
Cured Thickness per Ply (cm)0.022

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® M18/1 180°C Curing Epoxy Matrix
Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/40%/193P/CHS-3K
LATI LAESTRA G/40 40% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)

PHEXC183 / 98654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.