HexPly® M18/1 is a high performance, self extinguishing, tough epoxy matrix for use in primary aerospace structures. It exhibits low moisture absorption at saturation. HexPly® M18/1 is a toughened epoxy resin system supplied with unidirectional and woven carbon fibers. HexPly® M18/1 was developed as a controlled flow system to operate in environments up to 135ºC.Information provided by HexCel |