MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bethlehem Steel ASTM A529 Grade 42 3/16 to 1/2 in. thick, as-rolled steel plate  (discontinued **)
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: A low cost grade limited to 1/2 inch thickness, used occasionally for non-demanding applications.

The following are suggested consumables for arc welding processes for 0.476 - 1.27 cm (3/16 - 1/2 in.) thicknesses. For Manual Shielded Metal-Arc (AWS A5.5) use Low Hydrogen Electrodes E60xx, and E70xx. For Submerged Arc (AWS A5.23) use F6x-Exxx, and F7x-Exxx. For Gas Metal-Arc (AWS A5.28) use ER70S-x. For Flux Cored-Arc (AWS A5.29) use E6xT-x, and E7xT-x except -2, -3, -10, or -GS.

Information provided by Bethlehem Steel Corporation

Data published in 1997. Bethlehem Steel in no longer in business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccTypical of ASTM Steel
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 123 - 172based on conversion from tensile strength
Hardness, Rockwell B 69 - 87based on conversion from tensile strength
Tensile Strength at Break 60000 - 85000 psi
Tensile Strength, Yield >= 42000 psi
Elongation at Break >= 17 %in 8"
 >= 20 %in 2"
Bend Radius, Minimum 1.0 t≤3/4" W; ASTM A6 PARA. S14
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.27 %
Copper, Cu >= 0.20 %
Iron, Fe >= 97.84 %
Manganese, Mn <= 1.2 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 0.40 %
Sulfur, S <= 0.050 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A529 Steel
ASTM A36 Steel, plate
ASTM A36 Steel, bar
Bethlehem Steel ASTM A529 Grade 50 3/16 to 1 in. thick, as-rolled steel plate
ASTM A283 Steel, grade D

NBETH017 / 15376

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.