MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Trinseo PULSE™ XT70 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Product Description: PULSE™ XT70 is a very easy flow, high-heat, high gloss and low density PC/ABS resin, delivering optimized performance for automotive exterior component applications.
Benefits: High gloss and meeting exterior paintability requirements; Low density driving to lighter and cost optimized parts; Very easy flow, reduced scrap, and faster cycle times, while enabling thin wall part design for mass reduction; Heath resistance optimized for the majority of automotive exterior applications
Applications: Spoilers; Side mirrors; Front grills; Exterior trims

Availability: Asia Pacific; Europe; North America

Features: Good Surface Finish; High Flow; High Gloss; Medium Heat Resistance; Paintable

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim

Form: Pellets

Processing Method: Injection Molding

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmISO 294-4
Melt Flow 24 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 7260 psiISO 527-2/50
Tensile Modulus 341000 psiIOS 527-1/1
Charpy Impact, Notched 9.60 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 24.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 42.0 - 44.0 µin/in-°FISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 212 °FUnannealed; ISO 75-2/A
Vicat Softening Point 245 °FISO 306/B50
 
Processing PropertiesOriginal ValueComments
Melt Temperature <= 536 °F
Mold Temperature 140 - 176 °F
Drying Temperature 212 °F
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRINSE1542 / 312235

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.