MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo PULSE™ XT70 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Product Description: PULSE™ XT70 is a very easy flow, high-heat, high gloss and low density PC/ABS resin, delivering optimized performance for automotive exterior component applications.
Benefits: High gloss and meeting exterior paintability requirements; Low density driving to lighter and cost optimized parts; Very easy flow, reduced scrap, and faster cycle times, while enabling thin wall part design for mass reduction; Heath resistance optimized for the majority of automotive exterior applications
Applications: Spoilers; Side mirrors; Front grills; Exterior trims

Availability: Asia Pacific; Europe; North America

Features: Good Surface Finish; High Flow; High Gloss; Medium Heat Resistance; Paintable

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim

Form: Pellets

Processing Method: Injection Molding

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow 24 g/10 min
@Load 5.00 kg,
Temperature 260 °C
24 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.1 MPa7260 psiISO 527-2/50
Tensile Modulus 2.35 GPa341 ksiIOS 527-1/1
Charpy Impact, Notched  2.02 J/cm²
@Temperature -30.0 °C
9.60 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 5.04 J/cm²
@Temperature 22.8 °C
24.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 75.6 - 79.2 µm/m-°C42.0 - 44.0 µin/in-°FISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FUnannealed; ISO 75-2/A
Vicat Softening Point 118 °C245 °FISO 306/B50
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 280 °C<= 536 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 100 °C212 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRINSE1542 / 312235

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.