MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical Lutex 120 NBR Latex  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Tensile strength, Elongation, Oil resistance, Abrasion resistance, Excellent elasticity, Whiteness

Application: Nitrile Glove (Examination Glove, Clean Room Glove), Supported Glove (Industrial Glove)

CSA No. 9010-81-5 and 7732-18-5

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 44.5 - 45.5 %
@Temperature 130 °C,
Time 1800 sec
Dry residual gravimetric; LSY-QB-ID001
Particle Size 120 - 150 µmLaser Light Scattering Method; LSY-QB-ID016
pH 8.2 - 8.8LSY-XB-YD006
Viscosity <= 100 cP
@Time 60.0 sec
#60 spindle, 60 rpm; LSY-QB-ID006
Surface Tension 30 - 40 dynes/cmRing Type; LSY-QB-ID005
 
Descriptive Properties
Coagulum<50 ppmMesh (#200, >74 µm), LSY-QB-ID004

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Synthos DL 455 SB Latex
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Dow Latex XZ 92240.03 Experimental Latex
Avient Aquamix™ 568 Latex

PLAY237 / 148247

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.