MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Latex XZ 92240.03 Experimental Latex  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: Description: XZ 92240.03 Experimental latex is an aqueous dispersion of a modified carboxylated styrene butadiene copolymer. It has been developed for use as a precoat /adhesive latex for secondary backing of tufted carpet where a medium handle is required.

Applications: Precoating and Secondary backing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 50 - 51 %50 - 51 %
Particle Mesh Size 100 Mesh100 Mesh<0.1 g/l residues
 325 Mesh325 Mesh<0.2 g/l residues
pH 7.2 - 7.67.2 - 7.6
Brookfield Viscosity 50 - 350 cP50 - 350 cP#2 @ 50 rpm
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 2.00 °C35.6 °F
 
Descriptive Properties
Minimum film formation temperature<0°C
Styrene content in polymer58%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Synthos DL 455 SB Latex
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
LG Chemical Lutex 120 NBR Latex
Avient Aquamix™ 568 Latex

PDWST110 / 142319

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.